Composition(percentage by mass)
Ni |
Cr |
Co |
Ti |
Al |
Mo |
Ta |
Bal |
14.0-16.0 |
8.0-9.0 |
2.50-4.00 |
2.50-1-4.00 |
1.00-2.00 |
1.00-2.00 |
Ta |
Nb |
C |
Fe |
Zr |
B |
O |
1.00-2.00 |
0.50-1.50 |
<=0.15 |
<=0.10 |
<=0.10 |
<=0.15 |
<=0.01 |
category |