Supply Iron-based superalloy powder iron alloy powder 3D printing powder
category |
Alloy grades and characteristics |
Alloy number: |
Stainless steel:304,316L,410L,15-5PH,17-4PH,2Cr13; high-strength steel:A100,300M,30CrMnSiA,40CrMnSiMoVA; Work die steel:18Ni300,H13,M2,M35,M42,T15,2030,S390 Iron Nickel alloy powder:Invar 36 |
Particle size: |
0-20μm, 15-45μm, 15-53μm, 53-105μm, 53-150μm, 105-250μm |
Morphology: |
Spherical or nearly spherical |
Appearance: |
Grey |
Package: |
Aluminum bag,Vacuum packing |
Application: |
3D printing metal powder |
Other applications: |
powder metallurgy(PM), injection molding(MIM), spray painting(SP) etc. |
Alloy number |
Material forming process and state |
Mechanical property |
||
|
|
σb(MPa) |